first of all reaction on the previous message: pretty strange to see somebody react as it were alu castings when the questionner says it is SG iron. Oops...Monday morning syndrom? Alu camshafts, sounds pretty soft to me for that job...
Treatment in the ladle doesn't give perfect standarised solution for nodularisation. Possebilities are water content in the sand.