Dear Arun

The relation cromium and carbon is 10 /1.
The temperature optimum to heat treatment is 1010 C, but you must be care with heating velocity. This velocity is not superior a 85 C/ hr.
After air cooling is good to make a temper at 250 a 300C

Regards