Subject: Casting grids of Lead-Antimony Alloy is brittle .

Date: 10/16/03 at 4:19 AM
Posted by: bich nga
E-mail: hanchaubattery@hcm.vnn.vn
Message Posted:


We have some following problems about Lead-Antimony Alloy:
Casting grids of Lead-Antimony Alloy is more and more brittle and dark colour after 3 days.
What impurity elements in Lead-Antimony Alloy can cause this problem ?
Could you point out some reasons about this problems , and how to solve ,please ?
Iam looking forwards to hearing from you .