Subject: Re: Tapping from EAF

Date: 01/01/01 at 10:32 AM
Posted by: Dr Arun Rao
E-mail: kasc@satyam.net.in
Message Posted:

In Reply to: Tapping from EAF posted by Saltem on 12/08/00 at 3:52 PM:

What is the grade of steel you manufacture?. Before adding such strong deoxidizers, the practice is to add the mild ones like FeMn, FeSi, etc. Carbon addition will certainly have to be made depending on the grade to be manufactured. Then finally aluminium is to be added. In order to get clean steel your ladle metallurgy and also the ladle condition will also govern the end product.