Usually nihard 4 has hardness as cast.
If necesary more hardness you need to remove the alloys in solution in the matriz.
Heat at 800 C slowly 75 a 80 C
maintenance 1 hr more 1 hr for each 25 mm
cool slow until 500 C
Stress relieve 250 a 350 C

You need more information contact me

sorry my english is not good

Aguinaldo gonsalez