Subject: Re: A type graphite formation in Grey Iron

Date: 04/04/01 at 10:04 AM
Posted by: Dr Arun Rao
E-mail: kasc@satyam.net.in
Message Posted:

In Reply to: A type graphite formation in Grey Iron posted by Vikas Goel on 04/03/01 at 7:50 AM:

Ensure proper inoculation in order to get A type graphite all other factore being same. Normally 0.5% of propreitary inoculant addition will aid in getting required microstructure. Also look into the problem of inoculant fading,though this may not be as severe as in S.G Iron. Hope this helps