Subject: Re: Composition window of Russian Al-Sc alloys

Date: 02/04/03 at 10:54 AM
Posted by: Mario Guerra
E-mail: guerramr@yahoo.com
Message Posted:

In Reply to: Re: Composition window of Russian Al-Sc alloys posted by Jostein Røyset on 02/04/03 at 9:39 AM:

Thank you for your reply on these two alloys.

Do you by any chance know were can I find the compositions of these two alloys?

Russian alloy 1980 T1, and Russian alloy 1953 T1

What does the T1 Stands for? is this a temper designation for Peak strenght or Overgaed Condition?

I would appresiate your feed back.
Thank you in advance.

Regards,
Mario Guerra.