Subject: Re: Need of low outgassing/nonmagnetic material

Date: 08/14/03 at 9:06 PM
Posted by: Pat McMahon
E-mail: patmcmahon@earthlink.net
Message Posted:

In Reply to: Need of low outgassing/nonmagnetic material posted by Frank Sanders on 08/14/03 at 7:08 PM:

Frank,

At this pressure and temperature brass would be a poor choice as would aluminum. Look for 316 stainless and, if your budget allows, silver plate it to reduce galling.