Hi all,

¿Is there any correlation between NaOH test and Salt spray test for Al metallized and protected reflectors?
¿Could someone suggest me on how can I improve corrosion resistance from 30 min till 3 hours in NaOH 0.2% test?.
Parts are Al metallized and polymer silicone layer protected automotive reflectors or headlamps.
¿Does someone know about especifications for Corrosion and Humidity Test for automotive Reflectors?